Product Introduction
CS300M Potentiostat/Galvanostat contains a fast digital function generator, high-speed data acquisition circuitry, a potentiostat and a galvanostat. With high performance in stability and accuracy with advanced hardware and well-functioned software, it is an entery and cost-effective model. With methods such as Potentiodynamic (Tafel plot), it’s widely used to measure pitting corrosion potential.
International standards of pitting corrosion potential measurement:
China: GB 4334.9-84
USA: ASTM G61-1986(2014)
Japan: JIS G0577-1981
etc...
Standards
GB/T 17899-1999
GB/T 18590-2001
GB/T 32550-2016
Industry standards
YY/T 1074-2002
YY/T0149-2006
YY/T 0695-2008

Experiment setup


Software parameters' setting

Typical Pitting potential
Techniques
Techniques - CS300M
Stable polarization
· Open Circuit Potential (OCP)
· Potentiostatic (I-T curve)
· Galvanostatic
· Potentiodynamic (Tafel plot)
· Galvanodynamic (DGP)
· Sweep-Step Functions (SSF)
Transient Polarization
· Multi Potential Steps
· Multi Current Steps
· Potential Stair-Step (VSTEP)
· Galvanic Stair-Step (ISTEP)
Chrono Method
· Chronopotentiometry (CP)
· Chronoamperametry (CA)
· Chronocaulometry (CC)
Voltammetry
· Linear Sweep Voltammetry (LSV)
· Cylic Voltammetry (CV)
· Staircase Voltammetry (SCV)#
· Square Wave Voltammetry (SWV)#
· Differential Pulse Voltammetry (DPV)#
· Normal Pulse Voltammetry (NPV)#
· Differential Normal Pulse Voltammetry (DNPV)#
· AC Voltammetry (ACV)
· 2nd harmonic AC Voltammetry (SHACV)
· Fourier Transform AC Voltammetry (FTACV)
#There is corresponding voltammetry stripping methods
Corrosion Measurements
· Cyclic polarization curve (CPP)
· Linear polarization curve (LPR)
· Electrochemical Potentiokinetic Reactivation (EPR)
· Electrochemical Noise (EN)
· Zero resistance Ammeter (ZRA)
Battery test
· Battery Charge and Discharge
· Galvanostatic Charge and Discharge (GCD)
· Potentiostatic Charging and Discharging
· Potentiostatic Intermittent Titration Technique
· Galvanostatic Intermittent Titration Technique
Product Introduction
CS300M Potentiostat/Galvanostat contains a fast digital function generator, high-speed data acquisition circuitry, a potentiostat and a galvanostat. With high performance in stability and accuracy with advanced hardware and well-functioned software, it is an entery and cost-effective model. With methods such as Potentiodynamic (Tafel plot), it’s widely used to measure pitting corrosion potential.
International standards of pitting corrosion potential measurement:
China: GB 4334.9-84
USA: ASTM G61-1986(2014)
Japan: JIS G0577-1981
etc...
Standards
GB/T 17899-1999
GB/T 18590-2001
GB/T 32550-2016
Industry standards
YY/T 1074-2002
YY/T0149-2006
YY/T 0695-2008

Experiment setup


Software parameters' setting

Typical Pitting potential
Specifications
| Specifications |
| Support 2-, 3- or 4-electrode system |
Potential and current range: Automatic |
| Potential control range: ±10V |
Current control range: ±2A |
| Potential control accuracy:0.1%×full range±1mV |
Current control accuracy: 0.1%×full range |
| Potential resolution: 10μV (>100Hz),3μV (<10Hz) |
Current sensitivity:1pA |
| Rise time: <1μS (<10mA), <10μS (<2A) |
Reference electrode input impedance:1012Ω||20pF |
| Current range: 2nA~2A, 10 ranges |
Compliance voltage: ±21V |
| Maximum current output: 2A |
CV and LSV scan rate: 0.001mV~10,000V/s |
| CA and CC pulse width: 0.0001~65,000s |
Current increment during scan: 1mA@1A/ms |
| Potential increment during scan:0.076mV@1V/ms |
SWV frequency: 0.001~100 kHz |
| DPV and NPV pulse width: 0.0001~1000s |
AD data acquisition:16bit@1 MHz,20bit@1 kHz |
| DA Resolution:16bit, setup time:1μs |
Minimum potential increment in CV: 0.075mV |
| Low-pass filters: covering 8-decade |
Operating System: Windows 10/11 |
| Interface: USB 2.0 |
Weight / Measurements: 6.5kg, 36.5 x 30.5 x16 cm |
Techniques
Techniques - CS300M
Stable polarization
· Open Circuit Potential (OCP)
· Potentiostatic (I-T curve)
· Galvanostatic
· Potentiodynamic (Tafel plot)
· Galvanodynamic (DGP)
· Sweep-Step Functions (SSF)
Transient Polarization
· Multi Potential Steps
· Multi Current Steps
· Potential Stair-Step (VSTEP)
· Galvanic Stair-Step (ISTEP)
Chrono Method
· Chronopotentiometry (CP)
· Chronoamperametry (CA)
· Chronocaulometry (CC)
Voltammetry
· Linear Sweep Voltammetry (LSV)
· Cylic Voltammetry (CV)
· Staircase Voltammetry (SCV)#
· Square Wave Voltammetry (SWV)#
· Differential Pulse Voltammetry (DPV)#
· Normal Pulse Voltammetry (NPV)#
· Differential Normal Pulse Voltammetry (DNPV)#
· AC Voltammetry (ACV)
· 2nd harmonic AC Voltammetry (SHACV)
· Fourier Transform AC Voltammetry (FTACV)
#There is corresponding voltammetry stripping methods
Corrosion Measurements
· Cyclic polarization curve (CPP)
· Linear polarization curve (LPR)
· Electrochemical Potentiokinetic Reactivation (EPR)
· Electrochemical Noise (EN)
· Zero resistance Ammeter (ZRA)
Battery test
· Battery Charge and Discharge
· Galvanostatic Charge and Discharge (GCD)
· Potentiostatic Charging and Discharging
· Potentiostatic Intermittent Titration Technique
· Galvanostatic Intermittent Titration Technique
Download